posted on 2020-02-10, 14:01authored byRachael Greenhalgh, Vincent Tsai, Ali Abbas, Vlad Kornienko, Tom Fiducia, Mustafa Togay, K Li, Chris R.M. Grovenor, AH Danielson, Amit Munshi, KL Barth, WS Sampath, Jake BowersJake Bowers, Michael WallsMichael Walls
The treatment of CdTe with a CdBr2 activation annealing step has been performed and the device characterized for its electrical, compositional and structural properties with Capacitance-Voltage, Current-Voltage, Transmission Electron Microscopy, Energy Dispersive X-ray analysis (EDX), Electron Backscattered Diffraction Analysis, photoluminescence and high spatial resolution- Secondary Ion Mass Spectrometry (nanoSIMS). NanoSIMS and EDX show the bromine segregating in the grain boundaries and also in through grain defects. This CdBr2 treated sample has a net doping density of 1.05x1014 cm-3 , an efficiency of 8.6 % with a Jsc of 23.7 mAcm-2 and Voc of 762 mV. The bandgap has been calculated to be 1.49 eV
Funding
EPSRC Centre for Doctoral Training in New and Sustainable PV : EP/L01551X/1
History
School
Mechanical, Electrical and Manufacturing Engineering
Research Unit
Centre for Renewable Energy Systems Technology (CREST)
Personal use of this material is permitted. Permission from IEEE must be obtained for all other uses, in any current or future media, including reprinting/republishing this material for advertising or promotional purposes, creating new collective works, for resale or redistribution to servers or lists, or reuse of any copyrighted component of this work in other works.