posted on 2017-10-12, 10:02authored byRudolph Kashinga, Liguo Zhao, Vadim SilberschmidtVadim Silberschmidt, Farukh Farukh, N.C. Barnard, M.T. Whittaker, Daniela Proprentner, Barbara Shollock, G. McColvin
Low cycle fatigue (LCF) of a low-carbon (LC) directionally-solidified (DS) nickel-base superalloy, CM247 LC DS, was investigated using both experimental and computational methods. Strain-controlled LCF tests were conducted at 850°C, with a loading direction either parallel or perpendicular to the solidification direction. Trapezoidal loading-waveforms with 2 s and 200 s dwell times imposed at the minimum and the maximum strains were adopted for the testing. A constant strain range of 2% was maintained throughout the fully-reversed loading conditions (strain ratio R = −1). The observed fatigue life was shorter when the loading direction was perpendicular to the solidification one, indicating an anisotropic material response. It was found that the stress amplitude remained almost constant until final fracture, suggesting limited cyclic hardening/softening. Also, stress relaxation was clearly observed during the dwell period. Scanning Electron Microscopy fractographic analyses showed evidence of similar failure modes in all the specimens. To understand deformation at grain level, crystal plasticity finite element modelling was carried out based on grain textures measured with EBSD. The model simulated the full history of cyclic stress-strain responses. It was particularly revealed that the misorientations between columnar grains resulted in heterogeneous deformation and localised stress concentrations, which became more severe when the loading direction was normal to a solidification direction, explaining the shorter fatigue life observed.
Funding
The work was funded by the EPSRC (Grants EP/K026844/1 and EP/M000966/1) of the UK,
and in collaboration with GE Power, Dstl and Uniper.
History
School
Mechanical, Electrical and Manufacturing Engineering
Published in
Materials Science and Engineering: A
Citation
KASHINGA, R.J. ... et al, 2017. Low cycle fatigue of a directionally solidified nickel-based superalloy: testing, characterisation and modelling. Materials Science and Engineering: A, 708, (December 2017), pp. 503-513.
This work is made available according to the conditions of the Creative Commons Attribution 4.0 International (CC BY 4.0) licence. Full details of this licence are available at: http://creativecommons.org/licenses/ by/4.0/
Acceptance date
2017-10-05
Publication date
2017
Notes
This is an Open Access Article. It is published by Elsevier under the Creative Commons Attribution 4.0 International Licence (CC BY). Full details of this licence are available at: http://creativecommons.org/licenses/by/4.0/