posted on 2015-06-09, 10:29authored byDongbo Zhang, Shengkai Gong, Huibin Xu, Hongtao ZhangHongtao Zhang, Yafang Han
Ni3Al based alloy IC6, a high performance cast alloy with approximately 14 wt.% Mo addition, has been developed for turbine
blades and vanes of advanced aero-engines and other high temperature structural components. However, because of the high Mo
content, during high temperature use, Mo will diffuse into the protective coating layer, which will affect the thermal cycling
performance directly. In order to block the diffusion and improve the thermal cycling behavior of thermal barrier coatings (TBCs),
a Si chemical gradient MCrAlY–Si bond coat was prepared by changing the Si content from 0.35 wt.% at the interface of
substrate and bond coat to almost 0 near to the surface of the bond coat. For comparison, conventional two-layered structural
TBCs with MCrAlY as bond coat were also prepared. The fabricated coatings were evaluated for the microstructures and the
composition distribution properties, such as thermal stability and resistance to oxidation. For the bond coat without Si addition,
Mo content near the surface was higher than 7 wt.% after isothermal oxidation at 1373 K for 60 h and 12.5 wt.% after thermal
cycling tested at 1373 K for 300 h (600 cycles). However, in the Si chemical gradient bond coat, only 0.4 wt.% Mo was
detectable after isothermal oxidation at 1373 K for 100 h and approximately 0.66 wt.% after thermal cycling tested at 1373 K
for 340 h (680 cycles).
Funding
This research is sponsored by National Natural Science
Foundation of China (NSFC) and Specialized
Research Fund for the Doctoral Program of Higher
Education of China (SRFDP).
History
School
Aeronautical, Automotive, Chemical and Materials Engineering
Department
Materials
Published in
Surface and Coatings Technology
Citation
ZHANG, D. ... et al, 2003. Thermal cycling behaviors of thermal barrier coatings on intermetallic Ni3Al based superalloy. Surface and Coatings Technology, 168 (1), pp.78–83
This work is made available according to the conditions of the Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International (CC BY-NC-ND 4.0) licence. Full details of this licence are available at: https://creativecommons.org/licenses/by-nc-nd/4.0/