Cyclic deformation, fatigue crack initiation and crack growth in a nickel-based single-crystal superalloy

Download (24.3 MB)
thesis
posted on 2021-08-01, 00:33 authored by Lu Zhang
<div>Single-crystal nickel-based superalloys are dominantly used for turbine blades due to their superior mechanical properties, fatigue and creep resistance at elevated temperature. Typically, gas turbines operate at high alternating load during engine start-up and shut-down, which subjects nickel-based superalloys to severe cyclic loads in harsh environments. For gas turbine blades, a large proportion of service life is spent in the initiation and growth of short fatigue cracks. Therefore, it is important to understand the mechanism of cyclic deformation, crack initiation and the early stage of crack propagation for reliable service-life prediction and optimal design of gas turbine systems.</div><div>Cyclic deformation, fatigue crack initiation and short crack growth in nickel-based single-crystal superalloys have been studied experimentally and numerically in this thesis. Strain-controlled low-cycle fatigue (LCF) tests were carried out, with a focus on the effects of crystal orientation and temperature. [Continues.]</div>

Funding

Dislocation-Microstructure Interaction at a Crack Tip - In Search of a Driving Force for Short Crack Growth

Engineering and Physical Sciences Research Council

Find out more...

Oxidation Damage at a Crack Tip and Its Significance in Crack Growth under Fatigue-Oxidation Conditions

Engineering and Physical Sciences Research Council

Find out more...

History

School

  • Mechanical, Electrical and Manufacturing Engineering

Publisher

Loughborough University

Rights holder

© Lu Zhang

Publication date

2019

Notes

A thesis submitted in partial fulfilment of the requirements for the award of the degree of Doctor of Philosophy of Loughborough University.

Language

  • en

Supervisor(s)

Liguo Zhao ; Vadim Silberschmidt ; Anish Roy

Qualification name

  • PhD

Qualification level

  • Doctoral

This submission includes a signed certificate in addition to the thesis file(s)

  • I have submitted a signed certificate

Usage metrics

    Mechanical, Electrical and Manufacturing Engineering Theses

    Exports

    RefWorks
    BibTeX
    Ref. manager
    Endnote
    DataCite
    NLM
    DC