File(s) under permanent embargo

Reason: This item is currently closed access.

Microstructural evolution within mechanically and thermally degraded and rejuvenated nickel superalloys

thesis
posted on 2016-06-21, 15:35 authored by Andrew W. Rowe
Microstructural evolution within mechanically and thermally degraded and rejuvenated nickel superalloys

Funding

RWE

History

School

  • Aeronautical, Automotive, Chemical and Materials Engineering

Department

  • Materials

Publisher

© Andrew Rowe

Publisher statement

This work is made available according to the conditions of the Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International (CC BY-NC-ND 4.0) licence. Full details of this licence are available at: https://creativecommons.org/licenses/by-nc-nd/4.0/

Publication date

2015

Notes

This thesis is confidential until 30th September 2020. A Doctoral Thesis. Submitted in partial fulfilment of the requirements for the award of Doctor of Philosophy of Loughborough University.

Language

en