Multiscale modelling of nanoindentation

Download (14.29 MB)
thesis
posted on 2018-10-18, 09:24 authored by Edward McGee
The process of nanoindentation causes physical phenomena not only at the nano-scale, but at multiple length scales up to the macroscopic. This thesis investigates multiscale modelling of nanoindentation that links atomistic scale molecular dynamics (MD) to a finite element (FE) model in order to extend the length scales that can be modelled. Existing multiscale models are investigated and the relevant advantages and disadvantages of each are discussed. New coupling techniques are developed in both 2D and 3D, which are applied to nanoindentation test simulations to verify the models. A new force attribution 3D multiscale model is applied to some studies of nanoindentation of Au and Fe. The results are compared to those obtained through experiment and to atomistic only models to investigate the effect of the embedding continuum region. These studies show that by extending the length scales, long range effects of nanoindentation can be modelled in the far field by continuum mechanics giving results that are in closer agreement with the experiment. The new coupling method has wide application and a study of laser ablation of Au has been carried out to show that the multiscale modelling technique can be used to improve the description of this phenomenon also.

History

School

  • Science

Department

  • Mathematical Sciences

Publisher

© Edward McGee

Publisher statement

This work is made available according to the conditions of the Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International (CC BY-NC-ND 4.0) licence. Full details of this licence are available at: https://creativecommons.org/licenses/by-nc-nd/4.0/

Publication date

2006

Notes

A Doctoral Thesis. Submitted in partial fulfilment of the requirements for the award of Doctor of Philosophy at Loughborough University.

Language

  • en

Usage metrics

    Mathematical Sciences Theses

    Exports

    RefWorks
    BibTeX
    Ref. manager
    Endnote
    DataCite
    NLM
    DC